Suitable for material
(Click for material suitability)P
General construction steel / free machining steel
Material | <500 N/mm² | <700 N/mm² | <850 N/mm² | <1000 N/mm² | <1400 N/mm² |
---|---|---|---|---|---|
Suitability |
![]() |
![]() |
![]() |
![]() |
![]() |
P
Heat treatable steel
Material | <850 N/mm² | <1000 N/mm² | <1400 N/mm² | >1400 N/mm² |
---|---|---|---|---|
Suitability |
![]() |
![]() |
![]() |
![]() |
M
Rust and acid constant steels
Material | <700 N/mm² | >700 N/mm² |
---|---|---|
Suitability |
![]() |
![]() |
K
Cast iron and cast iron alloy
Material | Cast iron until 180 HB | Metallable cast iron | Cast iron with nodular graphite |
---|---|---|---|
Suitability |
N
Non-ferrous metal, plastics, graphite
Material | Aluminium und AL-alloyed until 6% Si | Aluminium und AL-alloyed (under 12% Si) | Aluminium alloyed over 12% Si | Copper, brass, bronze, red brass | Plastics - thermoplast | Plastics - duroplast | GFK/CFK | Graphite |
---|---|---|---|---|---|---|---|---|
Suitability |
![]() |
![]() |
![]() |
S
Special alloy and titanium
Material | Inconel, Hastelloy, Nimonic, Monel | Titanium |
---|---|---|
Suitability |
H
Hardened steel
Material | 45-55 HRC | 55-60 HRC | 60-65 HRC |
---|---|---|---|
Suitability |
available variants
E.2617.0.1100.500
11
11,0
500
450

alternatives
E.2617.0.1200.250
12
12,0
250
187

alternatives
E.2617.0.1200.315
12
12,0
315
235

alternatives
E.2617.0.1200.400
12
12,0
400
300

alternatives
E.2617.0.1200.500
12
12,0
500
450

alternatives
Cookie preferences
This website uses cookies, which are necessary for the technical operation of the website and are always set. Other cookies, which increase the comfort when using this website, are used for direct advertising or to facilitate interaction with other websites and social networks, are only set with your consent.